マイクロドロップ技術で吐出できる接着剤は次の通りです。
接着剤の種類
粘度
ノズル
温度
ディスペンシング特性
n.d.= データは有りません
mPas
L=事件
P=製造
紫外線硬化接着剤
Delo-Katiobond 4552
n.d.
n.d.
110
L
Delo Photobond 4403/1
105
n.d.
60
P
Delo Photobond 4435/1
400
n.d.
90
L
Delo Photobond 4302/1
100
n.d.
60
P
Dymax 136 M
90
25
55
P
Dymax 190 M
75
25
50
P
Dymax 401
70
25
45
P
Dymax 625 VLV
135
25
65
P
Dymax 628 VLV
100
25
40
P
Dymax 3086
130
25
60
P
Dymax 1-20426
70
25
44
L
Dymax 1-20271 VLV
100
25
77
P
Dymax 3-20256
1000
25
35
L
Loctite 302
100
25
60
P
Loctite 661
300-600
25
65
L
NOA 61
300
25
120
P
NOA 62
300
25
100
P
NOA 63
2000
25
90
L
NOA 68
5000
25
90
L
NOA 73
140
25
55
P
NOA 81
300
25
75
L
NOA 88
250
25
75
L
Optodyne 3000
n.d.
n.d.
90
L
UV OA-45
n.d.
n.d.
53
L
UVO 114
300-700
23
60
P
Vitralit 1505Li
400-500
n.d.
30
P
Vitralit 1705Li
n.d.
n.d.
75
P
Vitralit 6164
25
n.d.
30
P
Vitralit 9106
n.d.
n.d.
50
P
2コンポーネント接着材
Araldit D
1300-1800
25
67
P
Epo-Tek 301-2 A
n.d.
n.d.
70
L
Epo-Tek 301-2 B
n.d.
n.d.
24
P
Epo-Tek 353 ND A
n.d.
n.d.
70
L
Epo-Tek 353 ND B
n.d.
n.d.
60
L
Epoxonic 116A
n.d.
n.d.
68
P
Epoxonic 116B
n.d.
n.d.
40
P
Epoxonic 1033 A
900
n.d.
83
P
Epoxonic 1033 B
30
25
60
P
Haerter HY 956
370-470
25
75
P
Haerter HY 957
370-470
25
62
P
嫌気性接着剤
Loctite 290
12
25
25
L
Loctite 601
100
25
50
L
Loctite 648 UV
n.d.
65
50
P
ガラスシート上に紫外線硬化接着剤で作ったドロップのアレーです。構成は硬化した後にスキャニングされたものです。中心のドロップは5個のドロップでできています。 Uv_matri
merger マイクロドロップシステムは非常に精密で、空気中で異なった材料のドロップを合成することが可能です(特殊なアプリケーション)。これはシステムの優れた性能を示しています。